But the chemical properties have no remarkable influence on it ( 3 ) as the water - to - binder reduces wich is one of key factors in the perpormance of reactive powder concrete with steel slag, the fluidity decreases but the strength increases ; incorporation of 4 percent steel fiber in volume can decrease fluility and increase strength ; heat - curing benefits the increase of strength which can still develop in 28 day water curing after heat - curing
( 3 )水膠比是影響其性能最為關鍵因素之一,隨著水膠比的降低,流動性下降和強度的提高都很明顯;摻入4的鋼纖維對流動性的影響比較明顯,同時也不同程度地提高了強度;熱養護有利於強度的提高,經熱水養護後放置水中至28天齡期,其強度有較大提升,並沒有出現強度倒縮現象。 -
It is natural graphite as outstanding films phosphorus chemical processing, heat treatment, the non - pressure processing from any binder pure graphite products
它是由天然磷片石墨經特出化學處理、熱處理、壓力加工而成的不含任何粘結劑的純石墨製品。 -
Adjustment of the positioning of the binder molecules is feasible by means of site - directed immobilization via chemical modification of the carbohydrate chain ( 24, 28, 29 )
結合物分子位置可以用經碳水化合物鏈的化學修改的定點固定化方法來調節。 -
Formula s founded on factors of water - binder and fly ash content is feasible. at the same time , the effects of fly ash quality ( grade , fly ash from huaneng fuzhou power plant ), content of chemical admixture etc al, are investigated
本文利用環境掃描電子顯微鏡( esem )技術,研究粉煤灰對各齡期( 3d 、 7d 、 28d 、 60d )混凝土細觀結構的影響和不同品質粉煤灰對混凝土細觀結構的影響。 -
In this paper, in term of low water - binder ratio, high - volume fly ash concrete with chemical admixture is produced
本文採用雙摻(摻粉煤灰和高效減水劑) 、低水膠比的技術路線,配製高摻量粉煤灰混凝土。