拉伸性 的英文怎麼說

中文拼音 [shēnxìng]
拉伸性 英文
draftability
  • : 拉構詞成分。
  • : Ⅰ動詞(展開) stretch; extend Ⅱ名詞(姓氏) a surname
  • : Ⅰ名詞1 (性格) nature; character; disposition 2 (性能; 性質) property; quality 3 (性別) sex ...
  1. Atomistic simulation of tension properties of nano crystal copper wire under surface effects

    表面效應對納米銅桿拉伸性能影響的原子模擬
  2. One tends to develop a feeling that anything of a tensile nature is detrimental in fatigue.

    人們往往會有這樣的感覺;在疲勞中,一切具有拉伸性質的都是不利的。
  3. The tensile strength and young ’ s modulus of cf / ep specimens before and after vacuum thermo - cycling were measured by an electrical universal material testing machine. an electron scanning microscope was used to perform the surface morphology and fractography of specimens

    真空熱循環試驗前後cf / ep層合材料的拉伸性能由電子萬能材料試驗機完成,本文利用掃描電鏡觀測試樣表面形貌和后的斷口形貌。
  4. Test methods for tensile properties of carbon fiber multifilament

    碳纖維復絲拉伸性能試驗方法
  5. Investigation on the high strain rate properties of pva fiber bundles

    纖維束沖擊拉伸性能的實驗研究
  6. Textiles - stretchability of fabrics - determination of bagging of fabrics

    紡織品.織物的拉伸性.織物起拱的測定
  7. Method for evaluation of tensile properties of metallic superplastic materials using r - type specimen

    使用r型樣品測定金屬超塑材料拉伸性能的評價方法
  8. Atomic bonding and mechanical property of ai - mg alloy with trace zr

    合金的微觀組織和拉伸性能的影響
  9. Test method for tensile properties of glass fiber - reinforced plastics

    玻璃纖維增強塑料拉伸性能試驗方法
  10. Textiles - tensile properties of fabrics - part 2 : determination of breaking force - grab method

    紡織品織物拉伸性能第2部分:斷裂強力的測定抓樣法
  11. The intercalation mechanism of insitu emulsion polymerization has been proposed for the first time. then acr / montmorillonite nanocomposites blended with pvc, the tem and xrd indicated that the montmorillonite were dispersed with nanometer in pvc matrix. the flexural strength and flexure modulus of composites increased with the montmorillonite content, and the impact strength of composites a little increased

    且隨著acr蒙脫土納米復合材料中蒙脫土用量的增加,雖然pvc acr蒙脫土納米復合材料的拉伸性能變化不大,但抗彎強度和彎曲模量明顯增大,而且其缺口沖擊強度也有一定幅度的增大,具有工業實用價值。
  12. Test method for tensile properties

    擠玻璃纖維增強塑料桿拉伸性能試驗方法
  13. Test method for tensile properties of pultruded glass fiber reinforced plastic rods

    擠玻璃纖維增強塑料桿拉伸性能試驗方法
  14. Test method for tensile properties of carbon fiber strands

    碳纖維復絲拉伸性能檢驗方法
  15. Abstract : the fragile raw silk finished with softer or not and the normal raw silk are warped on the same beam and weaved. the number of end breaking and the tension of warp of different raw silk during weaving, as well as the tensile properties and dyeing behavior of fabric are compared and analysized. the results show : if the fragile raw silk is finished with softer, the number of end breaking during weaving will be obviously decreased, and the strength of fabric will be increased slightly, but the color deviation will be existed compared with the fabric made from normal raw silk

    文摘:將正常生絲、脆弱生絲、經柔軟劑處理的脆弱生絲一起作為經絲上機織造,比較它們織造過程中斷頭、張力情況,並對織物的拉伸性能、染色能作對比分析,結果表明:脆弱生絲經柔軟處理后斷頭次數明顯減少,織物強力有所增加,但與正常生絲一起染色存在色差。
  16. For fatigue life cycles test, when the reaction film resides at the area near the surface of specimen readily to initiate crack, and the fatigue life cycles were greatly deteriorated

    拉伸性質方面,試棒在相同應變速率下,試棒中反應膜面積率越多對試棒的強度及延率的影響越嚴重。
  17. Tensile behavior of composite laminates with one - side bonded repair

    單面貼補修理后層合板的拉伸性
  18. Our main products are flexible 8 copper bar, 2. 6 oxygen - free copper wire, 0. 4 - 2. 5 copper wire of various sizes, naked 0. 08 - 0. 3 copper wire and tinned wire, which meet the requirements of the clients of different aspects and different levels, especially in the recent years, the developed and introduced flexible 8 oxygen - free copper bar which adopts both electrolytic plate and shot copper as raw material, producing packable speedy draw0. 08 copper wire with characteristics, smooth in appearance, free in burs, good in flexibility and good in drawing, appreciated very much by broad clients

    主要產品包括8軟態銅桿14低氧銅桿2 . 6無氧銅線0 . 4 - 2 . 5各種規格銅線0 . 08 - 0 . 3裸銅線鍍錫線。滿足各方面各層次客戶的要求,特別近年開發引進8軟態無氧銅桿,除可用電解板為原料外更可採用進口優質銅米為原料。生產可包高速0 . 08銅線,該產品具有外表光滑無毛刺柔軟拉伸性能好等特點,深受廣大客戶歡迎。
  19. Method for determination of rheological properties ofdoughs using an extensograph

    面團拉伸性能測定法儀法
  20. Comparing with the traditional tensile test instrument of textile. the new testing instrument of longitudinal tensile simulates the conduit condition of the vascular prosthesis in vivo, so it is suitable for the test of longitudinal tensile mechanic properties of vascular prosthesis

    相對于傳統的紡織品的測試裝置來說,新設計的針對人造血管的軸向拉伸性能的測試裝置模擬人造血管在體內的圓柱體管道的狀態。
分享友人