木材儲量 的英文怎麼說

中文拼音 [cáichǔliáng]
木材儲量 英文
timber reserves
  • : Ⅰ名詞1 (樹木) tree 2 (木頭) timber; wood 3 (棺材) coffin 4 (姓氏) a surname Ⅱ形容詞1 (木...
  • : 名詞1 (木料) timber 2 (泛指可以直接製成成品的東西; 材料) material 3 (供寫作或參考的資料) ma...
  • : Ⅰ動詞(儲藏; 存放) store up; save; keep [have] in reserve Ⅱ名詞1. (繼承人) heir 2. (姓氏) a surname
  • : 量動1. (度量) measure 2. (估量) estimate; size up
  • 木材 : wood; timber; lumber; log; lignum木材廠 timber mill; 木材防蟲 wood protection against pest; 木材...
  1. Hongxing forestry is rich in natural resources, it has 15. 5million cubic meters of active timber reserves, in addition, it has more than one hundred kinds of trees such as korean pine, larch dragon spruce, fir, birch, oak and manchurian ash, etc, gold and iron, etc, many kinds of metal mines, such as abound in free burning coal, marble and limestone deposits ; hundreds of wild medicine materials with developing prosperity, such as acanthopanax, fruit of chinese magnoliavine and dangshen, etc

    紅星區自然資源相當豐富,活立總蓄積1550萬立方米,有紅松、落葉松、雲冷杉、樺、曲柳等百余種樹;黃金、鐵等多種金屬礦,長焰煤炭、大理石、石灰石等豐富,礦質優良;刺五加、五味子、黨參等幾百種野生藥頗有開發前景。
  2. In addition to this, in view of the rapid growth of china s economy, opportunities also appear for offering various types of services it, building and associated services, etc. to the chinese market

    拉脫維亞有著歐洲最富有的森林資源之一,森林覆蓋面積占國土面積的45以上,不斷增長的備總達5 . 5億立方米。
  3. The paper focuses on the processing technique of wood flour - recycle polystyrene composite, and assesses the effects of wood flour contents, coupling agent contents and the rotate speeds of extruder on water uptake, tension strength, bending strength and dynamic mechanical properties. the results can be shown as follows : with the increasing of wood flour, composites gain higher water uptake but lower dynamic mechanical properties, the storage moduli ( e " ) and glass transition temperature ( tg ) decrease

    較系統地研究了粉含、偶聯劑添加和雙螺桿擠出機的螺桿轉速等主要擠出工藝參數對復合料的吸水性能、拉伸強度、彎曲強度、動態機械性質(存e和損耗正切角tan )的影響規律,初步確定了適宜工藝條件,主要結論是: 1 )粉含的增加使得復合料的吸水性能增加,動態機械性質下降。
  4. Then tension and bending strength reach to maximum when the wood flour content is 40 %. the addition of coupling agent ( maleic - anhydried - modified polystyrene, maps ) can improve these properties described above

    當添加20的偶聯劑時,粉含為40和50的復合料的吸水減少了一倍;存高於未加偶聯劑的復合料;彎曲強度和拉伸強度分別增加了10和40以上。
  5. With 20 % coupling agent, composites with 40 % and 50 % wood - flour content gain better storage moduli ( e " ) than these without coupling agent, and composites with 40 % and 50 % wood powder content attain the increments in tension and bending strength of 10 % and 40 % respectively, the rotate speeds of extruder affect the mixing of wood powder, coupling agent and polystyrene

    3 )雙螺桿擠出機的轉速影響著粉偶聯劑和聚苯乙烯的均勻混合程度。研究發現,雙螺桿轉速為40rpm時,復合料性質好於其它轉速。 4 )粉含為40 ,偶聯劑含為20的復合料其力學強度(拉伸強度為40 . 22mpa ,彎曲強度為76 . 192mpa )和存明顯高於其他工藝條件的復合料。