Tips on welding of aluminized sheet in comparasion with cold rolled steel strip
鍍鋁鋼片的焊接狀態比較冷轆鋼片Abstract : for analyzing the residual stress distributing state within the weld joint, and its effect on the performance of welding structure, when welding the ferrite pearlite steel with the austenite steel, this paper develops a finite element program to compute the interface stress of two or over two material. finally, this program is used to analyze the mechanical behavior of heterogenic joint
文摘:為了分析鐵素體、珠光體類鋼與奧氏體類鋼焊接時,焊接接頭處焊接殘余應力的分佈狀態及其對焊接構件性能的影響,研製了可計算兩種或兩種以上材料界面應力的有限元程序,並用此程序分析了異質接頭的力學行為。Pre - data gathering module achieves the collection and communication of sixteen - route temperature signal. speed measuring and controlling module realizes the control of refolw soldering transfer speed by manipulating transducer. on - off outputting module fulfills calefaction control of calefaction tube by solid state relay. above position operator software programs by delphi, and realizes pid parameter automatic timing and no - oversnooting temperature control. software has friendly interface, convenient operation, complete functions
前置數據採集模塊完成16路溫度信號的採集和通訊;速度測量模塊與速度控制模塊通過控制變頻器來調節迴流焊的傳輸速度;開關量輸出模塊通過固態繼電器對加熱管進行控制;上位機軟體採用delphi編程,實現了pid參數自整定以及無超調的溫度控制。Isothermal superplastic solid - state welding of 4ocr and qcr0
5的恆溫超塑性固態焊接The comprehensive effect of partial acidlity of working medium, flowing status of fluid, nocuous material in atmosphere, together with the overlong usage, largely increased the corrosion rate and caused the leakage
結果表明,泄漏的主要原因是焊接缺陷導致焊縫區發生縫隙腐蝕,而工作介質的局部酸性、流體的流動形態、大氣中有害物質、溫差應力等綜合作用,加上使用期過長等加劇了腐蝕,導致該塔泄漏。Idea of differential plane is introduced in the calculation of orientation of normal line, and optimal orientation for electron gun is obtained. this work is helpful for guaranteeing welding quality
在法線姿態的計算中,引入微分平面的設計思想,獲得了焊接過程中的最佳姿態,保證了焊縫質量。Sanfeng electrical equipment co., ltd. is a professional manufacturer which products hf, solid hf, intermediate frequency, supersound frequency induction heating equipment, intermediate frequency overall anneal equipment and the installation of all - digital dc governor
經營高頻焊管全套設備及其配件保定市三豐電器有限公司是專業生產高頻固態高頻中頻超音頻感應加熱設備中頻整體退火設備和全數字直流調速裝置的專業廠家。Cavitation erosion and corrosion resistance of as - welded nickel aluminum bronze
焊態鎳鋁青銅的空蝕腐蝕性能When flux appears liquid and transparent on both tube and valve, start sweeping flame back and forth along axis of joint to maintain heat on parts to be joined, especially toward base of valve socket
當焊劑變成液態並且在管道和閥門上呈現半透明狀態時,開始將火焰沿著連接部件的軸線進行進退烘烤,以保持連接部件、特別是閥門套筒底座部位的熱度。If fluxed parts are allowed to stand, the water in the flux will evaporate, and dried flux is liable to flake off, exposing metal surfaces to oxidation
如果允許塗上焊劑的部件處于直立狀態,那麼焊劑中的水分會蒸發掉,而乾燥的焊劑很容易脫落,致使暴露的金屬表面容易被氧化。The analysis results indicate that the correlative influence factors to the technological capabilities of electronic solders include the composition and purity and chemical uniformity of solder alloy, the composition and properties of mother materials and their clean level on the surface, the surface tension of liquid state solders, the temperature and atmosphere in soldering and the activity of flux, the chemical composition and structure and properties of the surface film of melting solders, and so on
分析表明:相關的影響因素主要包括合金的組成、純度和化學均勻性;母材的成分、性質和表面的潔凈度;液態焊料的表面張力;釬焊溫度、氣氛、助焊劑的活性;液態焊料表面膜的組成、結構和性能等。But there are some technical difficults for the welding of aluminium alloy such as some broken bits being easily found, a large welding distortion can happen easily, hard to distinguish the difference between the solid metal and liquid metal colour, hard to control the temperature, a lot of air holes can be seen in the welding line and so on
但是鋁合金熔化焊時的技術難點在於:焊接時易引起夾渣,焊接變形大,金屬的固態和液態的色澤不容易區別,焊接操作時控制溫度困難,容易產生氣孔等等。如果焊前清理工作不是很好,檢測氣孔往往超標。Automatic planning of welding torch ' s gesture of arc welding robot
弧焊機器人焊槍姿態的自動規劃By compared with the simulation results and the experiment results, we come to the conclusions that : ( 1 ) circuit with assistant network can widen soft - switching extent in lagging arm, reduces duty - cycle loss on the secondary, diminishes switching dissipation of inverter spot - welding power source. ( 2 ) the range of resonant capacitor, the important factor to soft - switching process, not only affects zero - voltage turn - off of power switches, but also affects the range of zero - voltage turn - on of power switches. so resonant capacitors must be considered according to many aspects ; ( 3 ) it easily fulfils soft - switching condition in lagging arm as leakage inductance of power transformer increases, but bigger leakage inductance of power transformer increases opening dissipation of transformer and decreases efficiency of soft - switching inverter power source
通過模擬結果與軟開關點焊逆變器試驗結果的對比分析,得到了如下主要結論:採用輔助網路可以完全拓寬全橋軟開關逆變器的滯后橋臂軟開關范圍,減小了次級占空比丟失,降低了逆變電阻點焊電源的開關損耗;諧振電容是影響軟開關工作狀態的重要因素,其大小不僅影響開關管的零電壓關斷,同時也影響開關管的零電壓開通范圍,因此,諧振電容應該綜合考慮;功率變壓器漏感越大,越容易滿足滯后橋臂的軟開關條件,但是大的漏感也使變壓器的通態損耗增加,降低了軟開關逆變器的效率。Steel for the reinforcement of concrete. weldable ribbed reinforcing steel b500. technical delivery conditions for bars, coils and welded fabric
混凝土加固用鋼材.可焊接的混凝土加強鋼筋b500 .棒,環盤,已焊過的鋼筋網的交貨技術狀態Steels for welded round link chains ; technical delivery conditions
焊接的圓形鋼鏈用鋼材.交付技術狀態And it could shorten the time to build the body model and ensure the enough accurate rate on engineering. secondly, the methods to deal with the welded spots in this dissertation are used to build the fem model of biw ( body in white )
然後,將本文對車身焊點的處理方法應用到白車身有限元模型的建立中,其有限元模態分析結果與樣車的實驗模態分析結果吻合較好。Finally, a comparison experiment is performed between the speed regulating system this paper designed and the speed regulating system of nbc - 350 welding power source. the result indicates that the system this paper designed has good dynamic stability and control accuracy
最後,對本文設計的送絲機調速系統與nbc - 350焊機的調速系統進行了對比試驗,試驗證明本文設計的調速控制系統具有良好的動態穩定性和良好的控制精度。It is found that, the modes of coaxial optical emission of dissimilar gaps, clustering at distinct numerical range, can distinguish 1st, 2nd and 3rd class welds of different welding quality effectively
結果表明,同軸光信號幅值的眾數在不同間隙的焊縫段,聚集在線性可分的不同的區間,可以有效分開焊接質量不同的類、類、類焊縫;信號的分段功率譜分析能夠較為直觀地反映焊接狀態的變化。In this platform, the remote arc welding robot working environment is partitioned to macrostructure model and small area weld seam model. the macrostructure is defined to the position and gesture of basic makeup cell and it gets remote information from 3d geometry vision. the weld seam is a space curve and it gets information from structured laser sensor by user ’ s controlling
宏觀環境模型定義為基本組成單元在遠端的位置和姿態,本文通過現有的雙目立體視覺系統來獲取遠端環境典型特徵點的三維信息;小范圍焊縫模型定義為一條空間曲線,通過控制結構光傳感器運動,來獲取焊縫的三維信息。分享友人