粗選精礦 的英文怎麼說

中文拼音 [xuǎnjīngkuàng]
粗選精礦 英文
rougher concentrate
  • : Ⅰ形容詞1 (長條東西直徑大的) wide (in diameter); thick 2 (長條東西兩長邊的距離寬的) wide (i...
  • : Ⅰ動詞1. (挑選) select; choose; pick 2. (選舉) elect Ⅱ名詞(挑選出來編在一起的作品) selections; anthology
  • : Ⅰ形容詞1 (經過提煉或挑選的) refined; picked; choice 2 (完美;最好) perfect; excellent 3 (細)...
  • : 名詞1. (礦床) ore [mineral] deposit 2. (礦石) ore 3. (開采礦物的場所) mine
  1. In accordance with some wolfram - tin effuse come from cleaner in aconcentrating mill, this study adopt vibrate dslimes shaking table combining with centrifugal separator to put up a roughers. tousegravity - flotation and magnetic con - centration as combined proces s of technology, succeed in solving a problem of multipurpose returning in wolfram - tinslimes

    針對某廠廢棄的鎢錫溢流進行了試驗研究,採用振動泥搖床與離心機組合,運用重(水冶)聯合工藝流程,有效地解決了鎢錫細泥綜合回收問題。
  2. Combining the character of heiyingshan ' s lean iron ore and the experiences of hematite dressing home and abroad and locale character that located in the center of gobi desert and lacking electricity and fresh water, we have finished three ways of trial studying which are the magnetic ore dressing, lump dry - magnetic dressing and magnetic - gravity ore dressing

    根據黑鷹山貧鐵石性質和國內外紅鐵實踐,結合黑鷹山現場地處戈壁沙漠、缺電少水特點,擇全磁方案、塊-磁方案及磁-重方案進行試驗研究,針對試驗情況對中磁?強磁(一流程進行了擴大試驗。
  3. When the crude ore contains copper 1. 84 %, the technical indexes such as the grade of copper concentrate 22. 37 % and the recovery 78. 70 % are obtained by use of single - stage grinding, one time of roughing, three times of scavenging and two times of cleaning

    當原含銅1 . 84 %時,經過一段磨、一次、三次掃和二次,獲得銅品位22 . 37 % 、銅回收率78 . 70 %的技術指標。
  4. Abstract : the original mineral of dading iron mine was processed by the technique which included pre - classification, dry magnetic separation to discard dirt, magnetic separation of the coarsely ground ore, scondary grinding and secondary magntic separation of the rougher concentrate, thus raising the processing quantity of the crude ore, reducing the grinding cost, with the grade of iron concentrate 65. 54 %, the recovery of iron 94. 11 %

    文摘:採用預先分級、乾式磁拋廢、磨磁再磨再磁的工藝流程處理大頂鐵原生,提高了原處理量,降低了磨成本,獲得鐵品位65 . 54 、鐵回收率94 . 11的技術指標