細粉煤 的英文怎麼說

中文拼音 [fěnméi]
細粉煤 英文
fine coal
  • : 形容詞1 (條狀物橫剖面小) thin; slender 2 (顆粒小) in small particles; fine 3 (音量小) thin ...
  • : Ⅰ名詞1 (粉末) powder 2 (用澱粉製成的粉條或粉絲) noodles or vermicelli made from bean potato o...
  • : 名詞(黑色固體礦物) coal
  1. The excellent quality of coating film based on waterproof two - component polyurethane coating filled with fly ash can be gained when the fineness of fly ash is 300 meshes

    灰的度為300目時能得到性能優良的雙組分聚氨酯防水塗料。
  2. It focuses on the theory of the mineral functional materials " improving the anti - chloride permeability and the chloride binding. the main achievements of this article include : 1 ) use the technology of xrd, sem, bet, laser particle size distributor etc to test the component, the construction, particle size distributor, specific surface etc of micro - silica, ultra - fined slag, high quality fly ash, meta - kaolin clay, four types of the mineral functional material, theoretically analysis the functions which the four mineral functional minerals act on cement concrete, namely pozzolanicity effect, filling effect, micro - aggregate effect, surface adsorption effect and so bring into play the affect of plastification, lowing of temperature, reinforcement, improvement of durability. base on this analysis we can conclude that the proper diameter of the mineral functional material is 5 m - 15 m, that is blain fineness 4500cm2 / g - 7500cm2 / g

    本論文的主要成果包括以下幾個方面: ( 1 )採用xrd 、 sem 、 bet 、激光粒度分析儀等多種測試手段,探明了以硅灰,超磨粒化高爐礦渣,優質灰及偏高嶺土超等4種超礦物功能材料的組成、結構、粒度分佈、比表面積等基本性質;從理論上分析了礦物功能材料在混凝土中的4種效應,即火山灰效應、填充密實效應、微集料效應、表面吸附效應,並由此發揮出增塑、溫峰削減(降熱) ,增強及耐久性改善等作用;通過相關理論分析,推導出礦物功能材料的合理粒徑范圍在5 m 15 m ,即勃氏比表面積為4500cm ~ 2 g 7500cm ~ 2 g 。
  3. Critical velocity of ultra - fine comminuting coal with dia - jet

    前混合水射流超粒的臨界速度
  4. The secondary screens receive the coal from the crushers and remove the fines.

    經壓碎后的通過第二道篩,篩出
  5. Wearproof porcelain plate developed by this factory can be used as inside lining plate, coal delivery pipework, bin, bunker, separation port, wind pipe bend, exhauster, inner pipe of mill fan, air preheater, air fule and various dedust equipment for antifriction. besides, it can extend the service life of equipment

    耐磨瓷板系是我廠自行研製的適用於磨機內襯板,輸管道、料倉、料斗、粗、分離口、一、二次風管彎頭、引風機、排機內殼、空氣預熱器、尾部煙道等以及各類除塵系統設備的防磨抗蝕、延長設備的使用壽命。
  6. The expansion agents can only make up the shrinkage to some extent, and the compensation effects would be reduced when the retardener and fly - ash are used. the expansion agents are not panaceas to avoid the shrinkage cracking as expansion can also reduce the concrete soundness. under bad curing condition, the polypropylene fibrillated film fiber can improve concrete ' s anti - crarking property, while the nominal steels have very unobvious effects. to reduce the concrete shrinkage thus avoid the cracking, the former factors must all be taken into account in concrete proportion design to develop sound concrete

    研究結果表明,水泥的品種和用量是影響混凝土收縮值的主要因素之一,當混凝土中水泥用量超過470kg / m ~ 3時,混凝土的收縮值超過400 10 ~ ( - 6 ) ,在約束狀態下存在高開裂風險;採用砂使混凝土單位用水量顯著提高,收縮值也大幅增加;優質灰總體上能抑制混凝土的收縮,以超量方式摻入其抑制作用更加明顯,但灰混凝土早期的粘聚性較差,應注意養護,以免失水產生龜裂;早強減水劑和緩凝減水劑都會使混凝土收縮值增加;膨脹劑只能補償混凝土部分收縮,同時受緩凝劑和灰的抑制,而且膨脹使混凝土的體積安定性增加了不確定因素,膨脹劑不是解決混凝土收縮裂縫的良方。
  7. In this paper, the effects of fly ash, cement, lime, fine sands, foam agent, w / c ratio and additional agent on foamed concrete were studied by experiments, the best combination ratio of fly ash foamed concrete whose density varies from 551kg / m3 to 650kg / m3 was obtained through orthogonal test design, the foam agent quantity and the fly ash quantity effect the fly ash foamed concrete greatly, so the author selected them as independents to establish duality linear regression equations, the equations were quite ideal through the test of model summary r. moreover, the author also did some experiments about the water resistance of magnesium oxychloride cement fly ash foamed concrete, the outcome showed that phosphoric acid has good effect on water resistance, and its appropriate quantity was found

    本文通過試驗研究了灰、水泥、石灰、砂、發泡液、水灰比及外加劑對灰發泡混凝土性能的影響,採用正交設計試驗方法得出了600級灰發泡混凝土的最佳配合比,同時發現發泡液和灰摻量對發泡混凝土的影響最為顯著,因此,以二者為自變量建立了二元線性回歸方程,通過全相關系數的檢驗發現方程較為理想。此外,還對氯氧鎂水泥基灰發泡混凝土的耐水性進行了相關實驗,發現磷酸有較好的耐水性效果,同時找到了其合適的摻量范圍。
  8. Producing small building blocks by mixing modified levigation powdered coal into coal cinder

    改性磨細粉煤灰摻入渣生產小砌塊
  9. Based on in - situ investigation and laboratory experiments, the article analyzed in detail the factors which affect the transportation and strength characteristics of gangue cemented tailing grain fillings such as powder coal, water - reducer, mortar density and grain size distribution

    摘要以現場調查和室內實驗為基礎,從灰、減水劑、漿體濃度、粒級級配等方面,對矸石作為膠結充填骨料的管道輸送特性和強度特性進行了詳的分析。
  10. Study on combustion characteristic of micro - pulverized coal

    燃燒特性的研究
  11. The results show, the concrete produced by using pulverulent coal - fired ash has very nice durability

    結果表明,摻灰高強混凝土表現出優良的耐久性。
  12. All results show, the performance of the high - strength concrete with mixture of pulverulent coal - fired ash is higher than the standard high - strength concrete, and is increased significantly

    綜合研究結果表明,摻入磨細粉煤灰后的高強混凝土的各種性能均高於基準高強混凝土,得到了良好的改善。
  13. The results indicate that the all properties of pulverulent coal - fired ash are obviously higher than that if original coal - fired ash. based on the above studies, the studies on the strength changing mode of concrete with pulverulent are carried out. arrange of results are attained

    首先對比研究了磨灰與原狀灰在高強混凝土中的作用,結果表明,磨細粉煤灰的各種性能均好於原狀灰,這為下一步性能研究奠定了基礎。
  14. The concrete with the a 28 days compressive strength of c60 can be produced by using suitably pulverulent coal - fired ash, the higher the quantity of pulverlent coal - fired ash mixed in concrete with 10 % - 20 % is, the higher the strength of concrete is. then, we carry out the studies on the technics properties that reflect the comprehensive properties of concrete. we find that the separating and excreting water of the concrete can be avoided efficiently when the pulverulent coal - fired ash and superplasticizer are used suitably, the higher the quantity ration of coal - fired ash and super plasticizer are, the higher the caving degree of the concrete is

    在上述研究基礎上,對摻灰后混凝土的強度變化規律進行了分析研究,在適當配合比及高效減水劑的作用下,摻一定數量的磨細粉煤灰,在28天齡期可以配製出抗壓強度高於c60的狄高強混凝土;當磨細粉煤灰以10 - - 20不同的摻量分別摻入灰中時,灰高強混凝土的強度隨摻量的增大,各齡期強度均逐漸降低;在摻入8硅灰+ 10灰可使高強混凝土的各齡期強度都有很大增加,當單摻8灰時,混凝土的後期強度增加較快;灰混凝土必須加入高效減水劑遼十l彬技術人學碩十學位論文後j 」能達到高強的目的。
  15. The activatory coal gangue powder ( acgp ), ground cement clinker and natural gypsum are mixed by different ratios to prepare blended cement specimens, and its mortar compressive strength performance, water usage for standard consistency, and flowability of mortar are investigated

    摘要將經燃燒等過程進行活化處理的矸石與磨至一定比表面積的水泥熟料及天然生石膏混合均勻,製成了活化謀矸石摻量比例不同的多組混合水泥,並對其膠砂強度性能、標準稠度用水量、膠砂流動度進行了實驗檢測。
  16. Standard test method for sampling and fineness test of pulverized coal

    的取樣方法與度的標準試驗方法
  17. Influence of the pulverized flyash to the bulk stability of high - strength concrete

    細粉煤灰對高強度混凝土體積穩定性的影響
  18. Effect of the ground flyash to the anti - carbonization property of the high - performance concrete

    細粉煤灰對高性能混凝土抗碳化性能的影響
  19. In this paper, a series of ultra - fine fly ash composite powder ( cufa ii ) products for rapid repair are researched and developed successly with the ultra - fine fly ash as matrix. cufa ii can replace cement equivalently more than 30 %. high performance rapid repair concrete ( hprrc ) in which cufa ii replaces cement equivalently more than 30 % can meet the requirements of opening traffic within 12 ~ 48h, which solves the problem of opening traffic as soon as possible after damaged portland cement concrete pavement are repaired for a whole plate, and the engineering cost is lowered greatly

    本文以超細粉煤灰為基材,研製並開發出灰復合超快速修補專用摻合料( cufa )系列產品,等量取代水泥30 ,配製的高性能快速修補砼( hprrc )在12 48h內達到開放交通的要求,解決了破損的水泥砼路面整板翻修后快速開放交通這一問題,並大大降低工程成本。
  20. The main achievements in this paper are as following : 1 based on the systematical study about physical properties, particle morphologies and micro - mechanism of ultra - fine fly ash, cufa ii products are successly developed by means of optimizing the particle gradation and activation technique. hprrc composed of cufa ii products and with the strength grade no less than 32. 5r ordinary portland cement can meet the minimum strength index demands. at present, cufa ii has been produced commercially and applied to engineering

    本文主要研究成果如下: 1 、在系統研究了超細粉煤灰的物理性能、形貌、體效應微觀機理的基礎上,採用體優化組合、活化激發技術,復配的cufa產品與32 . 5r及以上的普通硅酸鹽水泥配製的hprrc可達到12 48h開放交通所需的最低強度指標要求;該產品己工業化生產並推廣應用。