  1. In order to realize the on - line prediction the baking temperature of ladle lining, and to study its temperature uniformity, a 3 - d transient mathematical model with multi - inlet and multi - outlet of ladle heating facility facilities was built

    摘要為了對鋼包的烘烤溫度進行在線預測,筆者耦合了流體流動、燃燒和換熱過程,建立了多入口、多出口的三維非穩態鋼包烘烤數學模型。
  2. Numerical analysis on temperature distribution of ladle lining using regenerative baker

    蓄熱式鋼包烘烤器鋼包內襯溫度分佈數值分析
  3. The results indicate that the regenerative ladle baking with high temperature air combustion techniquecan speed up ladle heating rate and increase the temperature uniformity of lining

    結果表明,採用助燃空氣煤氣雙預熱的蓄熱式燃燒技術能夠有效地提高鋼包的烘烤速度和加熱均勻性;氣體預熱溫度越高,包襯終點溫度越高,溫度均勻性也越好。
  4. Using cfx4. 3 code with finite difference and simplec methods, the temperature distribution of ladle lining baked at different preheating temperature of combustion gas was studied numerically and experimentally

    利用計算流體力學軟體cfx4 . 3 ,採用有限差分方法和修正的速度壓力耦合演算法simplec ,計算了某廠蓄熱式鋼包內襯的溫度分佈,重點分析了不同氣體預熱溫度下鋼包內襯溫度的變化規律,並進行了實驗驗證。
  5. Such measures as raising baking temperature of ladle, quickening thermal circulation of ladle, adding insulating lay in ladle lining, adding cover in molten steel surface, adding ladle cover in casting are introduced to reduce molten steel temperature drop in this paper

    闡明了通過提高鋼包烘烤溫度、加快鋼包熱周轉、包襯加隔熱層、鋼水表面加覆蓋劑、澆注鋼包加蓋等減少鋼水溫降的措施。
  6. The spraying mixes developed by our company for con - casting tudish working lining has good propertles of coating and long service life. it keeps working for one cast without eating away and leaking for average over 12 hours during the whole casting. when inversion casting the residual working lining can be easily disintegrated without sticking to the ladle and no powder coming from the disintegration, and also the working environment not polluted. meanwhile magnesia - calcium spraying mix has the functions of absorbing impurities in molten steel and pruifying molten steel

    我公司開發的連鑄中間包工作內襯噴塗(塗抹)料施工時塗抹性好,使用壽命長,在整個連澆過程中能持續工作一個澆次而不蝕漏平均12小時以上,用后在翻包時殘余工作襯能順利解體,不沾包、解體產物不粉化,不污染工作環境,鎂鈣質噴塗料還具有吸附鋼水雜質,凈化鋼水的作用。