nanoindentation 中文意思是什麼
nanoindentation
解釋
納米壓痕技術-
Gas permeability tester and mechanical folding device were developed to study the barrier property and deformation failure behaviors. the surface characterization, chemical structure, optical, mechanical properties of pet coated with dlc have been investigated by x - ray photoelectron spectroscopy ( xps ), contact angle measurement, light transmission analysis, nanoindentation and friction wear tests
通過x射線光電子譜分析、接觸角測定、光學透過率分析、納米壓痕、摩擦磨損試驗、機械彎折試驗、氣體透過率試驗,對膜層的表面特徵,光學、力學及氣體阻隔性能進行了系統的研究。 -
The tested materials include ( 100 ) silicon wafer, ( 110 ) silicon wafer, poly - silicon thin film, dry oxidized silicon dioxide thin film, wet oxidized silicon dioxide thin film, lto thin film, standard lpcvd silicon nitride film, low stress lpcvd silicon nitride film, alumni nitride film, zinc oxide film etc. in the nanoindentation experiment of the single crystal silicon, two different mechanical phases are observed at different indentation depth
用納米壓入法對( 100 )單晶硅及( 110 )單晶硅、多晶硅薄膜、干氧薄膜、濕氧薄膜、 lto薄膜、標準氮化硅薄膜、低應力氮化硅薄膜、氮化鋁薄膜、氧化鋅薄膜等重要材料的楊氏模量和納米硬度進行了系統地測量。報道了單晶硅在壓入過程中觀測到的兩個力學相的變化。 -
3d finite element simulation of the nanoindentation process
納米壓痕過程的三維有限元數值試驗研究 -
Nanoindentation and nanoscratch measurements on sub - micron tin coatings
亞微米氮化鈦膜的納米壓痕和劃痕測定 -
Nanoindentation technique is a technique that determines the mechanical properties of a material in the sub - micro scale
摘要納米壓痕技術是在亞微米尺度下決定一種材料機械屬性的測試方法。 -
This review mainly discussed the principle of nanoindentation and its current applications in wood science field
文中對納米壓痕技術的測試原理及其在木材科學中的應用現狀進行了較為詳細的論述。 -
Nanoindentation characteristics of ti - 12mo - 6zr - 2fe titanium alloy
鈦合金的納米壓入特徵 -
Mechanical properties of the electrodeposited nickel coating by nanoindentation
用納米壓痕法測量電沉積鎳鍍層的力學性能 -
The measurement of residual stress in electrodeposited nickel coating by nanoindentation
納米壓痕法測量電沉積鎳鍍層的殘余應力 -
Characterization of the surface roughness and nanoindentation hardness of au nicr ta multilayers
多層金屬膜的表面粗糙度和納米壓入硬度的研究 -
The results of finite element modeling are in good accord with the experimental data obtained from the nanoindentation and nanoscratching tests. it proved that fem is an effective method to analyze the deformation behavior of ti - dlc films
對ti - dlc膜的納米壓痕和劃痕實驗的數值模擬結果表明,有限元數值模擬是研究材料變形行為的一種有效手段。
分享友人