氣管發育不全 的英文怎麼說

中文拼音 [guǎnquán]
氣管發育不全 英文
agenesis of trachea
  • : Ⅰ名詞1 (氣體) gas 2 (空氣) air 3 (氣息) breath 4 (自然界冷熱陰晴等現象) weather 5 (氣味...
  • : Ⅰ名詞1 (管子) pipe; tube 2 (吹奏的樂器) wind musical instrument 3 (形狀似管的電器件) valve;...
  • : 名詞(頭發) hair
  • : 育動詞1. (生育) give birth to 2. (養活; 培育) rear; raise; bring up 3. (教育) educate
  • : 名詞[書面語] (剁物所用的木墩) a block of wood
  • : Ⅰ形容詞1 (完備; 齊全) complete 2 (整個) whole; entire; full; total Ⅱ副詞(完全; 都) entirely...
  • 氣管 : air tube; windpipe; trachea; weasand; tracheal sac氣管病 tracheopathy; tracheopathia; 氣管切開術 ...
  1. The influence of nano - al2o3 on the sintering and the properties of the si3n4 ceramics was researched in this paper. the samples with different amount of nano - al2o3 were obtained by using pressureless sintering at 1600, 1650, 1700 in the nitrogen atmosphere. the microstructure and the composition of the ceramics were determined by the means of x - ray, sem, micro - hardness meter etc. it is show that the sisty ceramics can be densified at 1650c to % percent of the theory density through the addition of nano - al2o3 ( the value could be 90 percent by other technique ). the crystalline growth of the cylindrical - si3n4 and the ratio of its longitude to its diameter are increased with the addition of nano - al2o3. a uniform microstructure and an fined crystal as well as more sialon phases can be obtained in the si3n4 ceramics through the addition of that

    實驗結果表明:在碳爐中、氮保護下進行燒結,添加劑為納米al _ 2o _ 3粉末時,由於納米粉末的高活性、高燒結驅動力,在1650就可使si _ 3n _ 4完地燒結,並使其緻密度可達理論密度的96以上(比其它工藝高6左右) ;同時,納米al _ 2o _ 3地加入大大促進了長柱狀? si _ 3n _ 4的生長和及柱狀晶長徑比的提高,使微觀結構均勻、細化,形成了更多力學性能優異的固體? sialon相,減少了利於陶瓷材料性能的晶間玻璃相,凈化了晶界。