martensite plate-
Combining with the results of implant test, the conclusion that the main reason of dropping the strength of austenite zone is the micro - crack located in the tip of flake graphite and marten site is drawn
結合插銷試驗結果提出了馬氏體相變過程中,在片狀石墨尖端及馬氏體組織中造成的微裂紋是奧氏體區強度下降並進而在外力作用下斷裂的主要原因。The lath width of martensite can be fined noticeably by pre - strained quenching at non - dynamic recrystallization to approach nanometer magnitude ( the average width is 120nm )
採用非動態再結晶溫度下的預應變-淬火,提高馬氏體相變形核率,可以超細化馬氏體的板條晶片寬度,使之接近納米量級水平(平均寬度達到120nm ) 。