stress-corrosion cracking 中文意思是什麼
stress-corrosion cracking
解釋
應力腐蝕開裂-
Standard test method for evaluating stress - corrosion cracking of stainless alloys with different nickel content in boiling acidified sodium chloride solution
沸騰酸化氯化鈉溶液中不同鎳合量不銹鋼合金應力腐蝕裂紋評定的標準試驗方法 -
Stress corrosion cracking of a batio3 ferroelectric ceramics
3鐵電陶瓷的應力腐蝕 -
Analyzed the reason of stress corrosion cracking on u shape brass tube bundle when it is having penetrative test with ammonia, improved technology of test and gave out the method should be paid attention to during the process of brass tube exchanger
摘要對黃銅管換熱器管束在氨滲試驗過程中發生應力腐蝕,導致銅管破裂的原因進行了分析,改進了施工方案,並提出了黃銅管換熱器製造過程中對管束進行耐壓試驗時的注意事項。 -
Standard test method for determining whether gas - leak - detector fluid solutions can cause stress corrosion cracking of brass alloys
測定氣漏檢測器液體溶劑是否能引起黃銅合金應力腐蝕斷裂的標準試驗方法 -
The failure analysis of the heating jacket indicates that the austenitic stainless steel 316l is susceptible to stress corrosion cracking under the combined action of chloride environment and residual stresses induced by welding
結果表明:加熱夾套開裂的主要原因是316l奧氏體不銹鋼不耐氯化物腐性,焊縫有一定的缺陷和腐蝕介質存在,屬於一種典型的應力腐蝕失效形式。 -
Standard classification of resistance to stress - corrosion cracking of heat - treatable aluminum alloys
熱處理鋁合金抗應力腐蝕斷裂性的標準分類 -
Standard test method for determining stress - corrosion cracking resistance of heat - treatable aluminum alloy products using breaking load method
用破壞載荷法測定可熱處理鋁合金製品的抗應力腐蝕開裂特性的標準試驗方法 -
Cqf product is mainly made of reinforced pp and all flow - through pump parts adopt injection mould with resistance to most organic and inorganic acid, alkali and salty solutions, applicable for being exposed outdoor with fine anticorrosive performance of stress corrosion cracking
Cqf型產品以增強聚丙烯為主要材料,泵的過流零部件均為注塑成型,能耐大多數的有機和無機酸、堿和鹽類溶液,也適于在室外大氣中暴露,對應力腐蝕破裂的抗蝕性良好。 -
Aerospace - space product assurance - material selection for controlling stress - corrosion cracking ; german and english version en 14101 : 2001
航空航天.航天產品保證.控制應力腐蝕裂紋材料的選擇 -
Corrosion of metals ; testing the resistance of metallic materials to stress corrosion cracking ; general
金屬的腐蝕.金屬材料耐應力腐蝕裂紋性能的檢驗.概況 -
Standard test method for determining susceptibility to stress - corrosion cracking of 2xxx and 7xxx aluminum alloy products
測定高強度鋁合金製品應力腐蝕斷裂敏感性的標準試驗方法 -
Stress corrosion cracking test for stainless steels
不銹鋼的應力腐蝕斷裂試驗 -
Test methods for stress corrosion cracking on aluminium alloys
鋁合金的應力腐蝕斷裂試驗方法 -
Effect of electrode polarization on stress corrosion cracking of 7075 aluminum alloys
電極極化對鋁合金應力腐蝕斷裂敏感性的影響 -
Space product assurance - material selection for controlling stress - corrosion cracking
航天產品保證.應力腐蝕斷裂控制用材料的選擇 -
Standard practice for evaluating stress - corrosion - cracking resistance of metals and alloys in a boiling magnesium chloride solution
評定在沸騰的氯化鎂溶液中金屬及其合金的抗應力腐蝕斷裂 -
Standard practice for evaluating stress - corrosion cracking resistance of low copper 7xxx series al - zn - mg - cu alloys in boiling 6 % sodium chloride solution
在6 %沸騰的氯化鈉溶液中進行鋁鋅鎂低銅合金的應力腐蝕斷裂試驗的標準實施規程 -
Standard practice for determining the susceptibility of stainless steels and related nickel - chromium - iron alloys to stress - corrosion cracking in polythionic acids
不銹鋼及有關鎳鉻鐵合金在連多硫酸中應力腐蝕斷裂靈敏性測定的標準實施規程 -
Current state of research on stress corrosion cracking in pipeline steels and damage mechanisms
管線鋼的應力腐蝕研究現狀及損傷機理 -
Testing of copper alloys ; stress corrosion cracking test using ammonia ; testing of components
銅合金的檢驗.用氨作應力腐蝕裂紋試驗.成分的檢驗